Fe-3%Si |
Fe-7%Si |
Fe50%Ni |
| Max Induction At 1000 A/m (12.5 Oe) [T] |
As Sintered Range |
1.45 |
1.33 |
1.4 |
As Sintered Mean |
1.45 |
1.33 |
1.4 |
Heat Treated Range |
1.5 |
|
|
Heat Treated Mean |
1.5 |
|
|
| Max Induction At 8000 A/m (100 Oe) [T] |
Heat Treated Range |
1.76 |
1.61 |
|
Heat Treated Mean |
1.76 |
1.61 |
|
| Residual Incuction [T] |
As Sintered Range |
1.35 |
1.25 |
0.42 |
As Sintered Mean |
1.35 |
1.25 |
0.42 |
Heat Treated Range |
1.4 |
|
|
Heat Treated Mean |
1.4 |
|
|
| Coercive Field [A/m] |
As Sintered Range |
54.5 |
29 |
9.4 |
As Sintered Mean |
54.5 |
29 |
9.4 |
Heat Treated Range |
41.8 |
|
|
Heat Treated Mean |
41.8 |
|
|
|